Standard Test Method for Determination of Susceptibility to Stress Corrosion Cracking in Copper Alloys Using an Ammonia Vapor Test

Archived
Yes
Incorporation
CFR Citation
46 CFR 56.01-2(e)(67)
Document Number
ASTM B858M
Document Edition
1995
Record Source
legacy system
SIBR Legacy Id
1785